S420N steel plate
S420N steel plate
We can supply ASTM:A572Grade50 A709Grade50 A588GradeB A633GradeD A633GradeE A573Grade58 A573Grade65 A573Grade70 EN10025:S420N, S420NL, S460N, S460NL Steel Plate Steel Plate ASTM:A283GrA S235JR S235J0 S235J2 SS400 SM400A St37-2 steel plates.If you are interested in chemical composition,mechanical property,and yield strength ,please send it to ,and i can give you the mill/quality certificate.The pressure vessel steel plate need high yield strength structure steel.
1.Commodity:EN10025:S355JR S355J0 S355J2 S355K2 S355NL low-alloy high-strength steel plates:
2.Referenced Standards:EN10025
3.Thickness*Width*Length: 8-250(mm)*1500-4000(mm)*5000-18000(mm)
4.Condition of Delivery: ImpactTest/Normalised/Quenched/Normalised+Quenched/HIC/Ultrasonic Test etc.
5.Date of Delivery: 20-50 days
6.Packing Condition: In bulk
7.Marking:The name of manufacture/brand/specification/steel grade/heat number/batch number
8.Order(min):2 pcs
9.Amoumt in stock:120 tons of each grade
10.Terms of Price:CIF/CFR/FOB/CNF
11.Terms of payment:T/T L/C
12.Port of Shipment:Shanghai Tianjin
If you need ASTM:A572Grade50 A709Grade50 A588GradeB A633GradeD A633GradeE A573Grade58 A573Grade65 A573Grade70 S420N, S420NL, S460N, S460NL Steel Plate STM:A283GrA S235JR S235J0 S235J2 SS400 SM400A St37-2 steel plates,or chemical composition,mechanical property,and tensile strength,Chemical composition % of the Product analysis of grade S420N (1.8902)Nominal thickness =< 63(mm) CEV max = 0.48
Nominal thickness from 63 to 100 (mm) CEV max = 0.50C Si Mn Ni P S Cr Mo max 0.22
max 0.65
0.95 - 1.8
max 0.85
max 0.03
Max0.025
max 0.35
max 0.13
V Nb Ti max 0.22
max 0.06
max 0.06
Temperature -20 -10 0 20 Notch impact test. Min. absorbed energy
40
43
47
55
Nominal thickness (mm) to 16 16 - 40 40 - 63 63 - 80 80 - 100 100 - 150 150 - 200 ReH - Minimum yield strength (MPa)
420
400
390
370
360
340
330
Nominal thickness (mm) to 100 100 - 200 Rm -Tensile strength (MPa)
520-680
500-650
Nominal thickness (mm) to 16 16 - 40 40 - 63 63 - 80 80 - 200 A - Minimum elongation Lo = 5,65 √ So (%)
19
19
19
18
18.
Germany DIN,WNr France AFNOR England BS Italy UNI China GB Russia GOST StE420
E 420 R
S420N steel plate We can supply ASTM:A572Grade50 A709Grade50 A588GradeB A633GradeD A633GradeE A573Grade58 A573Grade65 A573Grade70 EN10025:S420N, S420NL, S460N, S460NL Steel Plate Steel Plate ASTM:A283GrA S235JR S235J0 S235J2 SS400 SM400A St37-2 steel plates.If you are interested in chemical compo